    Cupronil, which i have used since its production began in the early
    seventies ( well, it was the seventies..who can remember anything
    exactly as it wasback then..!) has been a consistent, excellent
    performer as a firescale preventative and all around great flux
    product- particularly on silver work with many solder operations
    involved to fabricate a single piece..It has remained reasonable,
    affordable and is produced by an extremely reliable and well run
    business based on customer service and producing a top-quality
    product; rather than investing a fortune in advertising experience
    and word-of-mouth or passed down traditions are responsible for the
    continued consistency, reliability and availability of Cupronil. 

    It outperforms firescoff in both reliability, cost, ease of
    application and mechanism for delivery and other features ( like,
    and i hate to even type this - but toxicity..as firescoff has
    questionable aquatic effects not thoroughly researched as yet) that
    make it an essential consumable for my bench, and hence, my
    recommendation that everyone make it an essential on theirs as
    well...You will never be disappointed nor will you have to use an
    airbrush to apply it! 

    It is available in any size that suits your needs from a 4 oz. spray
    in unbreakable plastic to a gallon or larger if you have a
    manufacturing concern that is pumping fluids to a multi-bench set
    up.. 

R.E.Rourke


 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project