Thankyou,

    From all the replies I have had from this thread, I am now convinced
    that I have to try the 950 palladium as an alternate to plat...
    sounds like a good metal to be working in... As for the original
    problem... I made the ring set in white gold and used an 

    alloy of half silver half palladium. The colour was quite good, it
    worked well although it felt a bit more "sticky" than my usual mix. It
    was not quite as white as I hoped it would be and after explaining
    the rhodium to the client, 

    I ended up plating it anyway...I considered Ni. but decided against
    adding any just as a precaution. (I can't stand working nickel
    alloyed white gold) 

    Daniel, Raakhi, James, Lawrence, your info has been noted for future
    reference...Thanks. 

    Gwen. 

    (Just returned from a week in the bush unwinding and getting some
    fresh air... lots of elephant, lion, giraffe, zebra, buck and all
    the usual... such fun!!) 

 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project