>     At one extreme is platinum. We play our torch on the joint, the
>     heat stays near the joint but we need to get it really hot, so we
>     use a very hot but rather small flame. At the other extreme is fine
>     silver. The heat from our torch is rapidly conducted away to heat
>     up the entire work piece. The whole piece gets hot but our solder
>     flow point is much lower than the platinum example. For the silver
>     piece we need a fairly large QUANTITY of heat but not a really high
>     TEMPERATURE; with these requirements a tiny, super-hot flame can
>     get you in trouble much faster the a larger, cooler flame.
>     Think separately of TEMPERATURE and QUANTITY, it may help you (I
>     hope so). 

    This is why for any soldering operation on anything short of
    platinum or palladium I use a propane-compressed air torch with the
    appropriate sized tip (http://nationaltorch.com/3ab.html). Lots of
    heat at a manageable temperature. Little chance of firescale, or
    burning up all the flux or melting the work. Works from tiny tiny to
    teapot sized work. For casting I definitely use propane-oxygen but
    you have different requirements in needing to get the metal molten
    and cast as soon as possible. 

James Binnion
jbin AT mokume-gane.com
James Binnion Metal Arts
http://www.mokume-gane.com
360-756-6550


 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project