[Message Next]
[Thread Next]
From: Neilthejeweler Date: Fri Aug 10 00:39:21 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Your propane cylinder contains liquid propane. If the tank gets inverted at the correct angle the liquid covers the outlet in the torch head, extinguishing the flame. This is much more pronounced with a full or nearly full tank. I haven't tried one but there are little hosey thingies you can get to fit your tank, so that your tank remains upright and your flame stable. If you plan on getting more involved with jewelry I'd suggest you consider buying an oxy/propane setup with disposable bottles. You get a nice compromise...relative safety of small bottles and an excellent torch head with a wide choice of tips for small or large work. Not the cheapest route but its not crazy either. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project