>     I have never heard this and suspect that it may not be correct.
>     Both propane and MAPP are hydrocarbons and hydrocarbons are
>     generally compatible with each other. Also I have used the same
>     hose for MAPP and propane on my Bernzomatic torch for over 10 years
>     with no problem at all. Has anyone else ever heard this before? 

    The problem is that there are two types of fuel gas hose approved in
    the USA for use on torches Type R and Type T. Type R is used for
    acetylene and Type T is used for propane and other fuel gasses. The
    problem comes when you run propane in the Type R hose it will eat it
    and your hose will eventually fall apart. I have seen this happen
    with some of my hoses before I knew there was a difference and it is
    not an over night kind of thing but it does degrade it and make it
    brittle. So you should verify that the hoses you are using are rated
    for the fuel gas you are using. 

Jim

James Binnion
jbin AT mokume-gane.com
James Binnion Metal Arts
http://www.mokume-gane.com
360-756-6550
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project