Re: [Orchid] Using master alloys by themselves  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: Jeff Demand
Date: Fri Aug 03 03:02:58 2007
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

Adam,

    About 20 years ago one part of my job was making a sales line out of
    a 'master alloy' CZs and nice plating. Miserable stuff to work
    with... soft, tended to wick up solder, and turned my fingers green
    (far more so than copper brass, and bronze. Another consideration is
    that the coloured alloys depend on the gold for the final colour,
    they aren't coloured. A red alloy is mainly copper, green mainly
    silver, and both probably have small amounts of zinc and a few trace
    metals to enhance the final alloys intended use. Probably won't give
    the results you want but probably won't kill you either :-) The stuff
    is not expensive, buy a few ounces of each and experiment. Asking
    questions first is always a good idea but my most permanent learning
    came from first hand experience and experiments I lived through.

Jeff
Demand Designs
Analog/Digital Modelling & Goldsmithing
http://www.gmavt.net/~jdemand
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project