Allyson,

    It depends on what effect you want to achieve. If you want a nice
    burnishing and shine on the high points, stainless steel shot with
    water and a little dish soap works beautifully. Adjust the shape of
    the shot based on how deeply you want the burnishing to get into the
    recesses of your pieces. The larger and rounder the shot, the less
    "penetrating" it will be. 

    If you're going for more deburring (which seems unlikely if you've
    already gotten to the oxidizing step), ceramic media or charged
    plastic media (the little triangles) might work well. 

    Walnut shells charged with rouge can also work very well, but the
    size of the media is small enough that it will get into and
    abrade/remove the oxidation in recessed areas. 

Make sense?

Karen Goeller
No Limitations Designs
Hand-made, one-of-a-kind jewelry
www.nolimitations.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project