========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Noel MAPP gas will work just fine with silver I often use MAPP gas as a substitute for propane in my Bernzomatic torch as it burns hotter than propane. My Bernzomatic torch is the type that mixes the fuel with ambient air, so it is not very hot and MAPP gives it an extra boost. I have never tried MAPP gas in my Little Torch as the oxy/propane mixture is hot enough for the type of work that I do, but there is no reason that I can think of that would cause a problem with MAPP and silver in a Little Torch Regards Milt Calgary Canada ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project