>     after trying to have some sent from Hoover and strong- which is
>     only standard in wall thickness. 

    Sorry, that is not accurate. Although Hoover's on-hand stock is
    standard, you can request thicker or thinner walls. Hoover does
    require you to be quite size and thickness specific though. Just
    saying "thicker" won't get you too far. I order thicker walled tubes
    from Hoover for setting all of the time. Gives me more leeway in the
    stone sizes that I tube set. David Fell has thicker stock on hand.
    Hoover is a bit faster with the fabrication and shipping, but unless
    its an emergency, that shouldn't be a problem. Both companies are
    very reliable and helpful. 

    Lisa (What...?No Happy Birthday from anyone? Sheesh...where's my
    present Hans? Santa is writing things down. Went to the Autry Powwow
    yesterday. I might go today too!)
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project