Nisa,

    Jax Instant Silver Cleaner (not their regular silver polish) works
    fast on undesired patinas but cannot be used around pearls and
    probably shouldn't be used around softer stones such as opal (not
    sure, but I play that one safe). Most suppliers carry Jax products. 

    http://www.jaxchemical.com/jaxshop/shopexd.asp?id=89 

    SparkleSparkle Silver Cleaner is slower on heavy patinas (great on
    plain tarnish though) and can be used safely around any stone,
    including pearls. 

    http://www.nventa.com/sparklesparkle/-p-50.html 

    FYI SparkleSparkle's polishing cloths are the best polishing cloths
    I've ever used and quickly remove patinas and heavy tarnish in
    reachable areas. 

Victoria Lansford
http://www.victorialansford.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project