From: nick Date: Sat Jul 28 05:07:04 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Nickel oxidises to a green colour which stains the skin badly and is poisonous. It is also awkward to solder as it doesnt wet very well. It is very hard compared to silver. You can get cupro-nickel alloys (nickel silver, German silver) which are easier to work and will take solder well but unless you are practicing making boxes with interesting hinges I would recommend using copper instead as it is easier to work and to get hold of in most gauges of wire and sheet. You could always have you item plated if you require a silver finish. Bronze may be another choice for some finer work- see the thread on bronze alloys to obtain the grade you want. Nick ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project