Sandra, et al !

    Let me put some of my .02 scents worth in here.. ALL RINGS MUST BE
    PRE-POLISHED before setting. Now we got this all celared up, if I
    have to do any clean-ups after setting I would use a pumice wheel of
    180 grit, this leaves little labour for the 'polisher' afterwards. 

    Opals are soft and can loose their bevelled surface during the heavy
    polishing, but most ring polishers are very gentle with these
    stones.."most" is the clue word. I spend about 30% of my setting time
    in the 'full clean-up' everywhere..If I see any file marks they must
    be removed while at my bench, and not left for anyone else to 'polish
    off'. 

    Again in your case, I wold run a Flat or Tapered pumice wheel..(of
    your choosing) and check for any blemishes..then use a gentle Triploy
    and then a 'light' rouge afterwards!...BTW..silver is VERY SOFT and
    unforgiving 

Gerry!
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project