    I am not sure what properties are desired for bronze in jewelry
    making, but as someone who cast 90% of everything, but too long
    inactive, I would consider using shibuichi which is 50% silver and
    50% copper. Its color would be bronze/old copper when patinated. With
    the right chemical patina it may have several colors. I did not have
    good luck with "Baldwin's Patina" from REACTIVE METALS, are they
    still in business? Mine seemed not to work, and directions that if it
    were weak they said add copper-something-sulphate or such which if I
    had to begin with, I would not have bought their patina. It is very
    castable and should be rather good to work, though solder could be a
    problem. I don't know if higher silver content would lower or raise
    the temperature to make a solder, but it would be easy to find out. I
    did one project casting shakudo and was very pleased. I had a great
    shiny black patina on the piece and then decided to redo it, a
    frequent mistake I have of seeking perfection.....I used 10% 24k. I
    would very much like to do more mixed metal pieces and have several
    things that would work out rather well...if i do the work.... 

Jay
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project