Isolate definitely..!

    try leaving a margin of zoisite all around the cylinder..cleavage
    seems to be your disadvantage from what you described..the ruby in
    zoisite is more akin to a tourmaline crystal..and i completley agree
    with the copper and diamond lap recommendation.slow speed,cool as is
    possible cutting, and skip the 250 for something closer to 400 to
    start or look at some 3M products that have aggressive cutting
    capabilities with a webbed matrix of ceramic and diamond or ceramic
    and silicon carbide or zirconium..you can also just use a diamond
    wheel on a flexshaft ( continuous rimmed) at no more than 3500 to
    rough out your shape if its well lubricated with wintergreen oil,or
    synthetic methyl salicylate, or a product like liquid bur-lube to
    eliminate chipping,( reduce speed if you get any chatter)...I watched
    a guy at a "granite counter top " place cut a slab of it,followed by
    a slab of labradorite last Saturday..(by slab I mean 64"x 98" pieces)
    he had little chipping with a 60 inch saw blade he prepped with
    diamond spray and kept it wet and cool..the finished pieces were
    glass like with his copper and diamond polishing lap though he said
    he can get away with a polish like Linde A or cerium oxide on the
    ruby and zoisite... 

    a great reference is the international facetter's guild's
    archives..or the eclectic lapidary 

R.E.Rourke
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project