Re: [Orchid] Best Bronze for jewelry making?  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: DC
Date: Wed Jul 11 00:04:51 2007
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    Sorry I missed the original post but I have had good results casting
    with Caster's Brass Chunks, Caster's Bronze Chunks (white), and
    Ancient Bronze from Rio Grande. All of these can be melted in my
    electric melting furace. 

    When I worked at The Johnson Atelier (art foundry) we used Manganese
    Bronze, but I can't be more specific than that. 

    I really like the brass chunks and ancient bronze for casting, and I
    solder with high-copper wire solder to attach pin backs. Warning: the
    solder is silver in color. Also there is a blue/black patina that
    works well with the white bronze. 

Peace, Dave
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project