>     To say care is required might be a understatement for a substance
>     that cannot even be stored in a glass container. 

    I'm usually rather impatient with posts warning intelligent adults
    about the dangers of workshop chemicals, but I'll make an exception
    for HF. This stuff is not only dangerous but sneaky. If you contact
    it, you may not even know until hours later, when it's too late. HF
    burns may not be visible or painful, even while the HF is migrating
    to your bones and turning them into calcium fluoride. Specialized
    medications are needed even for first aid treatment. Read the linked
    MSDS. 

    http://www.bu.edu/es/labsafety/ESMSDSs/MSHydFluoricAcid.html 

    Al Balmer (who once spent half a day in the company clinic
    undergoing various unpleasant treatments because a few drops *might*
    have splashed on him.) 

Sun City, AZ
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project