From: Jan McClellan Date: Sat Jul 07 23:00:33 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Marianne, You can make one easily enough - just cut out the metal in the shape of a chevron, then roll up the "wings" tight enough to hold the cord but loose enough so the cord will slide when pulled. Solder the center to the center of the back of the bolo, up a bit so it will hang right. I do this with my silver bolos every time because I don't like the available spring gizmos which are usually made with base metal. I'll send a picture if my explanation leaves something to be desired - just let me know if you want one. BTW, your jewelry is out of this world - I've long admired your work. Jan www.designjewel.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project