Hi. Thanks for all your comments and advice.

    I'm thinking that the spring clasp on the 14k chain was the problem.
    I'm still stumped as to why the 14k didn't plate, only the 18k, which
    had a non-steel-interior bayonet clasp, not a spring clasp. Both
    clasps were submerged. WHY would the 14k clasp plate the neighboring
    18k chain, but not the chain it was attached to? A couple of you said
    that only the gold touching the steel would plate, but there was no
    steel touching the 18k. Yep, I'm seriously stumped. 

    Regarding old pickle, which a couple of people referred to, my
    pickle was not old, not blue, and had been used only a couple of
    dozen times previously. So I'm pretty sure that was not the problem. 

    So, now I'm going to take Cynthia's advice and mix up some hot
    H2O2/pickle solution and try again. Hopefully that will do the trick.
    I'll report back. 

Thanks again,
Sarah
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project