>     a friend of mine uses snake chain quite frequently and his method
>     is not to solder at all. He does it by sort of riveting the end cap
>     on. 

    I would be concerned that this might cause the snake chain to break
    at the rivet. 

    Here's a method I sometimes use: 

    Fit the end of the chain into a fairly snug piece of tube, then heat
    just the very end, and when hot, apply a largish snippet of solder.
    Then, after pickling, file the end flush-- it will look almost like
    solid silver-- and either drill through the tube and put a jump ring
    through, or solder a jump ring onto the end. Sometimes I hammer the
    soldered end of the tube to flatten it a bit before drilling. 

    The solder will not run up the chain far enough to emerge from the
    other end of the tube, but if in doubt, lay a piece of steel on the
    chain where it emerges from the tube, just to be sure. 

Noel
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project