    siliquar or soldering clay or investment to hold it all in place, and
    act as heat sink prevent reflow with correction fluid,or stop-flow(
    yellow ochre and alcohol), use a little piece of screen bent into a
    table shape ( about 2x2x 1/2") instead of big tripods over the
    charcoal block to reflect heat when sweating the hard solder and
    absorbing the cupric oxides to some degree put the textured bottom
    sheet between two pieces of fairly thin brass and give it a roll or
    two to flatten- worst case scenario texture is stretched out a bit OR
    use bottom sheet with slightly less flat surface as top sheet : more
    pattern,lays flat due to bottom sheet now being flatter.. gold solder
    requires higher temp than silver to attach gold bezel, so use yellow
    silver solder inside the bezel that has already been soldered with
    gold hard solder..
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project