Noel,

    I look at diamond files as indestructible, rough cutting files for
    both metal and stone. Now before all the skilled metalsmiths and
    bench jewelers start attacking me for using diamond files on metal I
    will agree that nothing cuts like a quality steel file. But a diamond
    file can be left out on the bench and subjected to a lot of abuse
    while quality metal files should be kept covered or in a drawer to
    protect them. Also, I like to have a diamond file handy if I come
    across a cab that doesn't have an even bevel and I'm too lazy to get
    up and walk over to the lapidary machines. 

    Also, diamond files cut bi-directionally where steel files only cut
    in one direction. So a student may pick up bad filing technique using
    diamond files. 

Rick Copeland
Silversmith and Lapidary Artisan
Colorado Springs, Colorado
http://home.covad.net/~rcopeland
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project