From: Terry Ogden Date: Sun Jun 10 06:37:09 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Tim I have a Lyman vibe unit, and one of the ones made for jewelry, a Raytech. One of the first things I noticed is the Raytech is quieter. My first Lyman lasted about 30 years I used it for reloading, the Raytech I have only had about 8. I still use a Lyman, a Midway and the Raytech. I tried wet work with the Lyman and it leaked. I placed and 'O' ring over the shaft and under the retainer nut, it worked, it doesn't leak, but I can hear it on the 3rd floor when it is running. I don't hear the Raytech and it didn't leak from the start. I use both the Lyman and the Midway unit for dry media now. You could probably tweak the Lyman to make it a flow through with little work. I would try a Midway unit though, it has a clear solid lid, rather than the strainer lid that comes on the Lyman. Terry ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project