From: John Burgess Date: Fri Jun 08 06:08:03 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > You suggest using distilled water to mix up the citric acid pickle. > * I'm thinking that the water collected from a dehumidifier would > work quite well. It is in actuality distilled - being condensed > from water vapor in the air... am I right John Burgess?? * G'day; Yes, quite right of course, but it will contain anything that had been airborne in the room; mainly bacteria and volatiles. If you have a supply of unchlorinated mains water that will be OK, or rain water (thats all we have at my house) However, citric acid is not so expensive that throwing it out when it starts to get scungy is a bad idea. I've always used battery acid, diluted a bit.-- Cheers for now, JohnB of NZ ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project