Hello Ian..

    their claim is that it's highly tarnish resistant, but doesn't cast
    well probably explains why they don't sell it in grain form.. I love
    Cooksons pre-fab dark yellow 22kt gold, and I used to buy quite a
    bit from the firm as i had a customer with an affinity for 9ct. gold
    and britannia serving trays..go figure- so while ordering i'd usually
    add a quantity of their 22kt DS sheet to my orders! However, I find
    Hoover and Strong in the US equally accommodating if not more so
    than Cookson, and H&S's de-ox silver is superior to the small amount
    of 1.2mm sheet I purchased from them to see how well it compared to
    the de-ox sterling. I don't really care for the argentium being sold
    under a few different names by a few manufacturers..as I use.999 and
    get along quite well with it for all silver needs.. As far as Zn
    fuming, i believe they are referring to quenching and
    soldering..releasing zinc is fairly easy when one heats an alloy
    containing it to the melting point..it's, i believe the first
    metal/element to burn off in an alloy.
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project