    I exclusively use fine silver when using silver at all (I like the
    properties of fine silver over sterling a thousand times greater.It
    doesn't oxidise becaue it has no copper, it's as forgiving a metal
    as 18 kt. gold and above,fuses without flux and eutecticly bonds to
    itself or "marrys" other metals beautifully in most applications. I
    find that paying a supplier for copper to be added is an unnecessary
    outlay-unless i'm in a hurry, or need massive quantities of it for a
    specific application. If i need sterling or "de-oxed "silver it's
    easy enough to manufacture myself!).. 

    What exactly do you need to know? If you can narrow your topic area a
    bit I'll be more than happy to share anything i've learned thus far
    about it with you.. Also what type of casting are you planning on as
    that narrows the topic area even further.. 

R.E.Rourke
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project