========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi all; I played the violin for years as a child, and there is no way, if you are using proper technique, that a ring would come in contact with the strings. The strings are depressed with the pads of the fingers. Also, violin strings aren't that rough. The lower strings are gut or nylon, wound with flat wire, the upper strings are smooth steel wire. Chording on a guitar would chew up a ring though. It sounds like this woman is just rough on her jewelry, and I think that such obvious wear and tear should relieve you of responsibility to repair the ring without charges. If it were my customer, I'd point out the damage, explain that jewelry is not designed to be exposed to harsh conditions, then offer to repair it free of labor costs if she agrees to pay for the materials. David L. Huffman ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project