Hi Gwen,

    It is most unlikely that the damage occurred as a result of playing
    the violin. For a start, the violin does not use steel strings -
    they wouldn't resonate under the bow. The strings are 'catgut' (dried
    sheeps intestines) or nylon. The are used with rosin which is
    abrasive but this is only applied to an area of about 2 inches in
    length below the bridge where the fingers don't contact them. In
    playing, the part of the finger on which the ring sits would not
    come into contact with the strings as the hand is arched so that only
    the fingertips touch the strings - any greater contact would damp the
    strings and stop them sounding. Unlike a guitar, there are no
    fingerboard frets which could possibly mark the underside of a ring.
    I think it is also unlikely that the stone loosened because of
    vibration - unlike my tuba where the low frequency vibrations rattle
    my tooth crowns loose every couple of years or so! I think I would
    look for another, more violent cause than music...... 

Best wishes,
Ian
Ian W. Wright
Sheffield UK
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project