>     I have done steam casting with the 2 inch cylinder (a small
>     item works the best)....I took a mayonnaise (large) jar lid,
>     punched a hole in it...put a screw up through the hole and made a
>     handle out of a 1 inch dowel about 4 inches long. Filled it full
>     with wet paper towels. When the cylinder was taken out of the
>     kiln, put it on a fireproof base....I slammed the lid with the wet
>     paper towels down on the open end and held it there until the steam
>     quit rising. This must have been in one of the publications
>     mentioned because I have been doing this for over 20 years. 

    Well ok but my question is I put flask in kiln melt out wax and get
    flask to temperature then remove it and melt the silver how? buy
    putting it in top of heated flask and returning to kiln? or torch I
    mean take it right out and slam it down where is the metal? 

    Confused sorry I need to master this technique as it is my last
    resort 

Teri
Silver & Cameo Heritage Jewelry
www.corneliusspick.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project