Dori

    1. Heat source
    2. Crucible to melt it in
    3. ingot mold
    4. Rolling mill

    Torch you have 

    Crucible, could be a lot of things, most common is the ceramic type
    for melting with a torch. Condition before use, i.e. coat with flux
    first and melt. 

    Ingot mold can be steel or a carbon block, just something to hold
    the shape of a basic plate form. 

    Rolling mill, make sure that your ingot is not thicker than what
    your mill will open to. Could hammer it down, but boy would you be
    along time, on the bright side, you would be an expert with a hammer
    after word. 

    Anneal often to keep your plate from cracking. 

    Alternative - get wax, a bar of soap piece of wood and carve to a
    design you want and then with cuttlefish bone press a mold into the
    surface and pour what you want. 

    I just hit the highlights of course, read the archives for specifics
    and additional alternatives. 

Terry
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project