    Have you tried the PUK2 welding system yet? What are you planning to
    do with it? Filling porosity in casting? Tack welding before
    soldering? Welding wires together? Etc,etc... Besides looking for an
    inexpensive way to buy one-please make sure if it will work for what
    you do in jewelry. 

    The PUK2 does many laser applications, but not all. Not only do you
    need the PUK2 itself, but many of the accessories are also needed. 

    See if there is someone near you who has one for you to work with.
    If not, let me know and perhaps we can work out some time for you to
    try it. We have one here and swear by it. Just couldn't justify the
    cost of a laser right now and this was a MUCH less expensive
    alternative. 

    I seriously doubt that you will find one at 50% of retail but good
    luck in your hunt. 

Best wishes,
Ruthie Cohen
Mountain Metalsmiths School of Jewelry & Lapidary
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project