Hi Jerry,

    I trust your rolling mill has grooves for the rolling of square
    bars. To get the longest wiRe: anneal the coin then cut it with tin
    snips spiralling in from the edge to as close to the centre as
    possible, the width of the strip you are cutting being about equal to
    the thickness of the coin. This gives you a rough square section
    wire. Straighten it with pliers and by tapping on the anvil, then
    roll it in the grooves of the rolling mill until it is uniform along
    its length, anneal, continue using the draw plate to get the wire
    diameter you want. This way the maximum wire diameter you can get is
    about 2/3 the thickness of the coin you started with. 

    I have managed to get thicker wire by cutting the spiral strip twice
    as wide as the thickness of the coin, then carefully rolling it so as
    to pinch the long axis in the rollers, and ending up with a wire
    diameter about the same as the coin thickness. 

Alastair
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project