========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I've used the Meco Midget for 14 years now. I use it with natural gas and oxygen. My preference is for the ventilated tips for more heat, and the little guys for bitty repairs. A few weeks ago, I began to use a new ventilated tip that I got from Otto Frei. I observed that the tips I have used for 14 years may have gotten dirty over time. I plunked the old ventilated tips in my sonic for a few minutes, blew them dry and they work exactly like the brand new one. I probably didn't need to buy new but now have the extras I may need in the future. Didn't Victor buy the Meco line? And then quit making the best torch I've ever used. I wonder how or who we could get to start making it again? I'm sure the little torch is great, but there is room for two, especially when so many of us still love the Meco after all these years. Does anybody here have good success with the little torch using residential pressure natural gas and oxygen? Specifically natural gas without a concentrator? Judy Hoch ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project