    A torch is a concoction of brass tubing that mixes two gases and a
    flame comes out the end. There has often been this recurring,
    "What's the best torch?" thing here on Orchid, but they are all just
    tubing that has a flame coming out the end. I've used just about
    every type of torch there is - they all gave me a flame - funny how
    that works. I've logged about 10,000 hours on the Mecco - it's
    comfortable, reliable, durable. What Alan says is largely true - the
    Smith Mini is fairly limited, and the Mecco can do the Smith's job
    and more. The Smith isn't limited by tips, it's limited by the
    tubing - there's only so much gas available through that 1/4"
    tubing. The point being, really, that I can make a flame with my
    torches that can solder 30 gauge wire, or I can get a flame that's a
    foot long - cutting torch, too, for that matter. It's not the
    handle, it's the flame. If you're content with the flame a mini
    torch give you, then you are. You're just not going to be making any
    men's belt buckles with it, but that's your prerogative, isn't it? 

http://www.donivanandmaggiora.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project