    My, Neil, aren't we ambitious! There are two ways to weld anything.
    There's what you might call light welding, where you put two pieces
    together and just fuse them. Then there's what you need to do -
    what's I believe called fillet welding. It is theoretically possible
    to just fuse your sizing, but for a good weld the metal should be
    actually fluid. If you do that with your job there's a good chance
    the weight of it will just make it slump or even drip off. What you
    need to do is have a triangular shaped space in the joint - miter
    one or both sides, somewhat. Then fuse it at the bottom of that
    space - I'd fuse one side in place and then go to the other side, so
    nothing moves - tack welding. Then fill that space with metal from
    the bottom up, making sure that everything flows well as you go. In
    other words, don't expect to just melt the whole seam at once, just
    make a puddle and then fill it more and more with platinum rod. When
    you file it down, if there's some pits just use a tiny bur to clean
    them out and then re-fuse them. It's going to be tricky and hot..... 

http://www.donivanandmaggiora.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project