    As I understand, you have plain platinum band with cross-section
    5mmx3mm. 

    If you want to increase the size by adding a piece, one way to do it
    would be to open ring to the required size and using torch and thin
    wire to fill the gap by melting small amounts of metal and fusing 
them
    with the ring a bit at a time. In this way you do not even have to
    cast a sizing section, and it would guaranty solid fusing through out
    the cross-section. It would be like sculpting using the torch. If you
    never did it before, practice on some scrap prior. 

    That said, I do not understand why the ring is not stretchable. You
    should be able to increase the size of the ring by careful forging
    with cross-peen hammer. Try to anneal the ring before stretching it.
    Remember, to anneal platinum, one must bring it to bright orange and
    keep it at that temperature for at least 30 seconds. 

Leonid
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project