========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Grace, I fuse my fine silver bezels because I like the way it looks, nice and clean. I also do it for enamelling purposes so that I don't have to worry about the bezel solder contaminating the enamel. I do not however fuse my bezels to the backing primarily because of the difficulty factor of fine silver to sterling silver. I always pickle regardless whether I use flux. Pickling makes sure that your surface is clean of grease and any other impurities. So, yes I pickle between and at the end of whatever I am fusing and/or soldering. I fuse fine silver links for chains all the time. I have been told, but haven't tried yet, that you can fuse argentium very easily. But, again you still need to pickle to get the greases of your work. Jennifer friedman Ventura, CA ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project