    Thanks Ken! I tend to be conservative, especially with small
    endmills. 

    So 1/32" 2 flute HSS endmill 

    3 ipm feed, 10,000 rpm and.010" depth of cut. I used the same
    feedrates for the titanium ones I've been doing. The drag engraving
    can go faster, I usually bump it up a bit. 

    You could probably go much faster, but as they say, slow and
    steady...I did accidentally program some gear earrings at 10 ipm and
    they cut fine but raised a bigger burr. As it is now the cut has a
    minimal bur and is easy to clean up. Also the silver chips kind of
    pile up and are easier to reclaim, although my mill is very sparkly
    right now. 

    For the titanium I used plain water as coolant as I didn't want the
    tape to let go. I cut the silver dry. 

    I've been having a lot of fun with the methods since I posted that.
    When I sell one pair on Etsy, I can just whack out another in short
    order. I also found that the double sided tape holds wax pretty well,
    who would have thought? (That was for a job with a.010 carbide
    endmill....) 

Nick
www.cartertools.com/nfhome.html
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project