    The trick to making a box, is to make two L shaped sides and then
    fit them together to make either a rectangular box or square. To file
    a straight line at the bend. I measure ( 3 times ) score (3 times )
    using a T square to make sure that I am lining things up at 90
    degrees. This makes fitting the triangle file into the groove easy.
    Charles Lewton Brain turned me on to using a L shaped joint
    reinforcer that you can find at any hardware store. It is small, so
    setting up the 90 degrees is easy. 

    After making your two L shaped sides and soldering the 90 degree
    bend together, then measure exactly one of the sides and make sure
    that one of the two sides on the corresponding piece is the same
    measurement. Slide them together, making the box shape rectangular or
    square- depending on what you want and solder those together. 

    Hope this is clear enough, and works for you 

Good Luck
Joan
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project