From: chris mead Date: Thu Feb 15 05:23:11 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Bryan, Channel setting is fairly simple providing you follow a few basic rules. Measure the length of the stones touching girdle to girdle for thechannellength.You need a reasonable amount of metal for each wall (each side) of at least .75mm,for your stone size i reckon a ring width of 3.5-4.0 mm if you want it to last.Then drill a straight channel to a diameter just a tad smaller than the stones and cut yourself a thread both sides with a sharp graver about.5mm down from the surface.If you time it right the stones should just slip in with a little "clicky" feel,then tighten with downward pressure and clean up. Job done!.The theory is dead simple and the actual work can be too,but there is a very fine line between just right and big trouble. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project