>     to describe it); so the 2-part RTV mold-making material I tried
>     won't work... or perhaps I should say, I'd never used this stuff
>     before, and I ended up with a coarse rubbery mess when I and the
>     result were "done" (as recommended by the vendor from whom I
>     purchased the stuff, 

    It sounds like either 

    a) your RTV stuff wasn't mixed properly -- i.e. not equal amounts,
    not mixing well enough or 

    b) it's old 

    I'd say you're on the right track, buy a new batch of RTV 2 part
    silicone mold making material, and try again. 

    If you'd asked what to use for this project, that's what I would
    have said. 

    The paint on stuff is a pain to work with and tears easily. 

    I don't quite get what you're molding. Is it an old lead printing
    block? 

    Let's see, what are your other choices? Polymer clay, that would not
    get as much detail as the silicone RTV. 

    Any reason why you can't work directly with the stamp? 

    You could print the stamp with ink on paper and have a rubber stamp
    made at Ready Stamps for $30.00. 

Good luck,

Elaine

Elaine Luther
Metalsmith, Certified PMC Instructor
http://www.CreativeTextureTools.com (TM)
Hard to Find Tools for Metal Clay
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project