From: James Binnion
Date: Sat Feb 10 07:04:03 2007
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>     Jim, Are you an alchemist? 

    no just too damn curious for my own good :-) 

>     My question, is the alcohol they sell in liquor stores ( Ever
>     clear) 100% drinkable stuff the same as what you are going to
>     experiment with? 

    The alcohol I have ordered is reactively pure isopropyl alcohol,
    basically the same stuff as in rubbing alcohol but no added water.I
    have never tried isopropyl for this purpose so I am curious if it
    will hold boric acid in solution. I have used methanol (wood
    alcohol) and ethanol (denatured alcohol) they both work but methanol
    holds more boric acid in solution. The problem with methanol is it is
    too toxic for me to feel comfortable with using it in the studio in
    the quantities that I use fire coat. So I stick with denatured
    ethanol as the safer if less effective solution. 

    Ever-clear is relatively pure ethanol probably 198 + proof or 99%
    pure, certainly a good candidate for use in fire coat preparations.
    It is a lot more expensive than denatured due to the federal taxes
    on drinking alcohol. 

Jim

James Binnion
jbin AT mokume-gane.com
James Binnion Metal Arts
http://www.mokume-gane.com
360-756-6550
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project