If you have tools with a very light coating of rust or light
pitting, a pencil eraser can do wonders. It isn't the solution to
all rust problems, but worth a try, especially because there's
usually a pencil close at hand. This solution is nontoxic and
doesn't damage the tool. My dad collected firearms and he used this
trick to remove light rust without damaging the bluing on the
handgun.