Hi Noel,

    Yes, the germanium in the alloy combines with oxygen to create
    germanium oxide. The germanium oxide does not let oxygen through,
    thus preventing tarnish and firescale. 

    In terms of your question "what do we need the "standard" alloy
    for?" I think, from what I've seen with the few pieces that I've made
    with it so far, I'll be using AS 970 rather than AS 925 when AS 970
    becomes more readily available. 

    As for other people....heck, I have no idea. Argentium Sterling is
    less expensive than 970 Argentium Silver, since it has less silver.
    So far, that's the only downside I see. It is really very little more
    money, though--on line, 970 AS is only 20 cents more per troy ounce
    than 925 AS. 

Cindy
Www.cynthiaeid.com
Cynthia Eid
http://www.cynthiaeid.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project