Re: [Orchid] Times and temps for heat treating gems?  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: John Sexton
Date: Thu Jan 04 06:09:08 2007
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    Jeanne : I will be interested in seeing if you different responces
    than I got when I asked this question.To paraphrase: The people that
    know won't tell you and besides why do you want to do that. Are you
    trying to cheat people by enhancing stones? Some of my answers where
    off list some onlist but the above was the condensed replys. I too
    had some Amethyst I want to play with. It was a lower grade from
    California and I wanted to see what could be done. In researching
    this issue I am finding that it is more than just temperatures and
    time. Some stones seem to require different gasses in the
    environment. Normal air might cloud the stone or burn it but Argone
    might give you a stable color change. I too have not found any
    specifics and have even searched about 300 books that supposedly
    gave this kind of info. All to find that they did not give the info
    claimed. Good Luck and if you do fing something please share it with
    me either on list or offlist. 

John (Jack) Sexton
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project