========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi All, If there is one mystery about working on a piece of jewelry, it's how to finish it properly and professionally. Ann Cahoon is a graduate of North Bennett Street School and is a professional goldsmith. She works in palladium white gold, 22K and 18K setting pear shaped diamonds, etc. Metalwerx is offering a workshop in the one area that everyone should know, including me! I plan to shoot some photos and have her write up an article for Ganoksin on this very workshop. However, in the meantime, this one is a don't miss. Final Finish: Tips and Tricks Instructor: Ms. Ann Cahoon Date: : 20 January 2007 - 21 January 2007 Read more at: http://www.metalwerx.com/workshop/199 Release those unfinished projects from your drawer and move them to polished perfection. You will learn tricks for soldering while retaining a mirror polish, tighten wobbly stones and revitalize stale designs. M E T A L W E R X School for Jewelry and the Metalarts 50 Guinan St. Waltham, MA 02451 781 891 3854 www.metalwerx.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project