Christel,

    The lid is rusting because of its reaction with the nitric acid. As
    long as you don't splash the liquid around and into your eyes, there
    is little or no danger in piercing the lid further, creating a hole
    large enough to pour the (now probably very weak) acid out. You can
    use a plastic bucket of cold water, into which you have dissolved
    four tablespoons of baking soda; simply pour the contents of the jar
    into the bucket, while stirring the liquid into the bucket. 

    In all likelihodd, the acid has probably long since broken down and
    does not present an extreme hazard. 

    If you are that concerned about this material, why not soak an old
    towel in the solution you made for the bucket, invert the jar on the
    towel and the jar's contents will seep into the towel, then you can
    simply hang it to dry then discard it. 

    An open jar of nitric, even weak nitric, will corrode everything
    ferrous within many feet of the source. Never store any acid or
    alkali in a container with a metal lid. 

    Incidentally, once neutralized or even strongly diluted with water,
    the nitric will cause no harm to the environment as it breaks down
    into simply Nitrogen and Oxygen. 

    Again, for safety's sake DO NOT add water to this container. 

Wayne

 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project