    The bottom line is that an ultrasonic loosens the dirt and cleans the
    jewelry. The steam machine will just blast off Whatever it can but if
    the dirt is old crud it tends to stay put. I worked for years using
    only an ultrasonic and rinsing with hot water... It is nice to have
    both but there is no comparison in cleaning ability of a good
    ultrasonic. Both have there place. 

    For under 300.00 you can pick up a good ultrasonic with heat.
    Steamers are more expensive...I use a steammaster. The important
    thing with the steamer is get one with an auto shut off when it runs
    out of water or you'll burn up the coil. 

    Also, someone else posted the steam takes time to come up to
    pressure which is why I didn't use mine for years. The ultrasonic you
    can fill with hot water and cleaning solution and are ready to go.
    (Dawn works well...Ultra CR from stuller works great!) 

Mark
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project