Hello Pablo;

>     Hello, my name is Pablo, I am from Argentina, in this country
>     there is not good flux for soldering silver, all they crystallize 

    If you can't order flux from one of our U.S.A. suppliers such as
    Stuller or Rio Grande, you can make a flux yourself that will work
    OK, but it's not quite as good as the kind you buy. First, you need
    to find Borax. Grocery stores carry 20 Mule Team brand borax in their
    laundry products. Potter also use it in their glazes, so if you know
    a potter, perhaps he or she could spare some. You will need to grind
    it very fine with a mortar and pestel, which is like a small version
    of the old tool used to grind corn for flat breads. (I see your
    English is quite good, but I can't know how large your vocabulary of
    English words are). I don't know much besides English and French.
    Anyway, once you get the borax ground fine, mix it with water to the
    consistency you prefer. Let us know if you try this, and whether it
    works for you. I'm sure others here will offer more suggestions.
    Best of luck. 

David L. Huffman

 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project