From: Aaron Schnur
Date: Thu Nov 30 05:27:59 2006
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

    Hi, I am an intermediate jeweler who has studied under a master
    jeweler for about three years. I am in the process of seting up a
    home studio and I am having trouble finding instruction on how to
    properly set up and use a torch system. Most acetylene supply places
    are not hands-on and will be passive about offering advice on what i
    should do. The safety handbook says I should be properly trained in
    safety procedures before operating a torch system although I have
    been using an acetylene and air setup at the school where I was
    trained for three years now. It works fine for the kind of stuff I
    do (mostly classical-not much soldering). I am finding out new facts
    about acetylene every day that I wouldn't have known to avoid that
    frighten me into thinking I am going to cause an explosion (such as
    the do not set on its side rule). With my last torch system I had
    large flames jutting out the side off the handle every time I
    extinguished the flame (not the little adorable ones that are usual
    but huge mushrooms). Of course the people who work at acetylene
    supply houses will not take a look at this as they mostly deal with
    large propane orders or heavy duty undersea welders rather than
    acetylene/atmospheric air jewelry crafters. I do not know anyone in
    the gas business. What extra equipment do i need to buy?; all I have
    now is a torch, no. 1, 2 tips, b tank, flashback arrestor, hose,
    single dial regulator... I have been making jewelry and soldering
    for a long time, the main issue is SAFETY. I just want to make sure
    that I am doing everything right. 

 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project