Hello Annabel,

    I did without an ultrasonic for a long time. How to best remove
    polishing compound relates to the nature of the compound. Soap and
    water will work, but is tedious. 

    There are a couple compounds advertised as removable with dish soap
    and water, and they do clean off more easily. However, the usual
    compounds are better removed by soaking in an ammonia-based liquid,
    followed by scrubbing with an old toothbrush. I've used straight
    ammonia (which can damage some stones), but the fumes are obnoxious.
    "409", "Mean Green", "Awesome" are tradenames for cleaners that have
    been good removers for me. As noted previously, some stones are
    sensitive to ammonia, so keep turquiose, lapis, pearls, etc. out of
    those liquids with ammonia. 

    Ultrasonics are a very nice thing to have, so plan to save your
    loose change and buy a good one eventually. Maybe put it on your wish
    list for your birthday or special event. My hubby hates to buy me
    tools, but that's my favorite gift. :-) 

Hope this helps,
Judy in Kansas, where we'll hopefully see some thunderstorms today! I
finished putting in my spring bulbs, so timing is perfect.

 
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project